Conductive · energy storage
Battery conductive carbon black and SWCNT for lithium-ion electrodes
Conductive carbon black SP13 and SP42, and single-walled carbon nanotube dispersions SC10 (cathode) and SA40 (anode), for LFP, NCM / NCA, graphite and silicon electrodes.
Conductive carbon black: SP13 and SP42
| Item | Unit | SP13 | SP42 |
|---|---|---|---|
| Application | — | Cathode & anode | Cathode & anode |
| NSA | m²/g | 65 ± 7 | 140 ± 10 |
| DBP | ml/100 g | 200 ± 20 | 150 ± 10 |
| Ash content | wt % | < 0.1 | < 0.1 |
Stable conductivity, good dispersibility, low ash, low grit and low metal content.
SWCNT dispersions: SC10 and SA40
| Item | Unit | SC10 | SA40 |
|---|---|---|---|
| Application | — | Cathode | Anode |
| SWCNT content | wt % | 1.0 ± 0.1 | 0.4 ± 0.04 |
| Total solid content | % mass | 3.0 ± 0.3 | 1.0 ± 0.1 |
| Dispersing agent | wt % | 2.0 | 0.6 |
| Solvent | wt % | 97.0 | 99.0 |
| Viscosity | cps | < 5,000 | < 2,000 |
High conductivity, high surface area and low metal content.
Starting points by electrode system
| Electrode | Budcon materials to evaluate |
|---|---|
| LFP cathode | SP13 · SC10 |
| NCM / NCA cathode | SP13 · SC10 |
| Graphite anode | SP13 · SP42 |
| Silicon / SiOx anode | SP42 · SA40 |
Typical values. Electrode performance depends on active material, binder, solvent, mixing and calendering; cell-level qualification is required.